Aloi ya Fe-Cr-Al yenye uwezo wa juu wa kustahimili uwezo na halijoto ya kuhudumia kuliko ile ya aloi ya NiCr na pia ina bei ya chini. Maombi:
Umeme wa Ironr-chrome-aluminium esistorstipis hutumika sana kutengeneza vifaa vya kupasha joto vya umeme katika vifaa vya nyumbani na vifuniko visivyo vya kawaida, vifaa vya pid ni pani za mafuta, mashine za ioni, hita, uundaji wa plastimoulding hufa, pasi za kutengenezea, vipuli vya chuma vilivyofunikwa na cartridge. Maudhui ya Kemikali Nyenzo za aloi | Muundo wa kemikali |
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Wengine |
upeo(≦) |
1Cr13Al4 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 12.5-15.0 | - | 3.5-4.5 | Pumzika | - |
0Cr15Al5 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 14.5-15.5 | - | 4.5-5.3 | Pumzika | - |
0Cr25Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 23.0-26.0 | ≦0.60 | 4.5-6.5 | Pumzika | - |
0Cr23Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 20.5-23.5 | ≦0.60 | 4.2-5.3 | Pumzika | - |
0Cr21Al6 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 19.0-22.0 | ≦0.60 | 5.0-7.0 | Pumzika | - |
0Cr19Al3 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 18.0-21.0 | ≦0.60 | 3.0-4.2 | Pumzika | - |
0Cr21Al6Nb | 0.05 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 21.0-23.0 | ≦0.60 | 5.0-7.0 | Pumzika | Nb kuongeza0.5 |
0Cr27Al7Mo2 | 0.05 | 0.0025 | 0.0025 | 0.2 | ≦0.40 | 26.5-27.8 | ≦0.60 | 6.0-7.0 | Pumzika | |
Daraja | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 |
Utungaji mdogo% | Cr | 12.0-15.0 | 22.0-26.0 | 23.0-26.0 | 19.0-22.0 | 22.5-24.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 5.0-7.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 |
Re | fursa | 0.04-1.0 | fursa | fursa | fursa | fursa | fursa | fursa |
Fe | Bal. | | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. |
| | | | | | | Nb0.5 | Mo1.8-2.2 |
Kiwango cha juu cha halijoto cha kufanya kazi (°C) | 650 | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 |
Ustahimilivu 20℃(Ω/mm2/m) | 1.25 | 1.48 | 1.42 | 1.40 | 1.35 | 1.23 | 1.45 | 1.53 |
Uzito (g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 |
Uendeshaji wa Joto kwa 20℃,W/(M·K) | 0.49 | 0.49 | 0.46 | 0.48 | 3.46 | 0.49 | 0.49 | 0.49 |
Mgawo wa Upanuzi wa Mstari(×10¯6/℃)20-1000℃) | 15.4 | 16 | 16 | 14 | 15 | 13.5 | 16 | 16 |
Takriban Kiwango Myeyuko(℃) | 1450 | 1520 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 |
Nguvu ya Mkazo (N/mm2) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 |
Kurefusha(%) | ›16 | ›10 | ›12 | ›12 | ›12 | ›12 | ›12 | ›10 |
Kiwango cha Kupunguza Utofauti wa Sehemu(%) | 65-75 | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 |
Mzunguko wa Kupinda Mara kwa Mara(F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 |
Ugumu (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 |
Muundo wa Micrographic | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite |
Mali ya Magnetic | Sumaku | Sumaku | Sumaku | Sumaku | Sumaku | Sumaku | Sumaku | Sumaku |
Maisha ya Haraka(h/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 |
Iliyotangulia: Waya ya NiCr 80/20 ya Kunyunyizia Joto kwa Kunyunyizia Arc: Suluhisho la Utendaji wa Juu Inayofuata: Aloi ya Nickel Hastelloy C276 Ernicrmo-4 Welding MIG TIG Welding Inconel C-276 C22, B3, B2 Waya