FECRAL 23-5/waya wa joto wa joto/waya wa gorofa
Inatumika hasa kwenye heater, inapokanzwa na kontena, nk.
NICR 80/20, NICR 70/30, NICR 60/15, NICR 35/20
Fecral15-5, fecral20-5, fecral 25-5, nk…
Constantan, alloy 30, aloi 60, aloi 90, nk.
Urekebishaji wa umeme kutoka 0.02 U ohm/m-1.53 u ohm/m
Fanya joto kutoka 200 C hadi 1400 C.
PLS kuwa huru kuwasiliana nasi ikiwa kuna swali lolote.
Nicr:
Resistohm 20, resistohm 30, resistohm 40, resistohm 60, resistohm 70, resistohm 80
Fecral:
Resistohm 125, resistohm 135, resistohm 140,
Resistohm 145, Resistohm 153
Cuni
Constantan, Cuprothal 5, Cuprothal 10, Cuprothal 15, Cuprothal 30, Eurica
Daraja la aloi ya fecral | Muundo wa kemikali % | |||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Re | Wengine |
max (≤) | ||||||||||
1CR13Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 12.5-15.0 | —- | 3.5-4.5 | 0.1 | Bal. |
0CR15Al5 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 14.5-15.5 | —- | 4.5-5.3 | 0.1 | Bal. |
0cr25al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | 0.1 | Bal. |
0cr23Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | 0.1 | Bal. |
0cr21al6 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
0cr21Al4 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 21.0-23.0 | ≤0.60 | 3.0-5.2 | 0.1 | Bal. |
0cr21al6nb | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
0CR27Al7MO2 | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | 0.1 | Bal. |
Muundo wa kemikali na mali:
Mali/daraja | NICR 80/20 | NICR 70/30 | NICR 60/15 | NICR 35/20 | NICR 30/20 | |
Kemikali kuu Muundo (%) | Ni | Bal. | Bal. | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | Bal. | Bal. | Bal. | |
Max inafanya kazi Joto (ºC) | 1200 | 1250 | 1150 | 1100 | 1100 | |
Resization saa 20ºC (μ ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Uzani (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Utaratibu wa mafuta (KJ/M · H · ºC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Mgawo wa mafuta Upanuzi (α × 10-6/ºC) | 18 | 17 | 17 | 19 | 19 | |
Hatua ya kuyeyuka (ºC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Elongation (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Muundo wa Micrographic | austenite | austenite | austenite | austenite | austenite | |
Mali ya sumaku | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic |
Daraja la Cuni Alloys | Urekebishaji wa umeme (20degreeΩ mm² /m) | mgawo wa joto wa upinzani (10^6/digrii) | Wiani g/mm² | Max. Joto (digrii) | Hatua ya kuyeyuka (digrii) |
Cuni1 | 0.03 | <1000 | 8.9 | 200 | 1085 |
Cuni2 | 0.05 | <1200 | 8.9 | 200 | 1090 |
Cuni6 | 0.10 | <600 | 8.9 | 220 | 1095 |
Cuni8 | 0.12 | <570 | 8.9 | 250 | 1097 |
CUNI10 | 0.15 | <500 | 8.9 | 250 | 1100 |
Cuni14 | 0.20 | <380 | 8.9 | 300 | 1115 |
Cuni19 | 0.25 | <250 | 8.9 | 300 | 1135 |
Cuni22 | 0.30 | <160 | 8.9 | 300 | 1150 |
CUNI30 | 0.35 | <100 | 8.9 | 350 | 1170 |
CUNI34 | 0.40 | -0 | 8.9 | 350 | 1180 |
Cuni40 | 0.48 | ± 40 | 8.9 | 400 | 1280 |
Cuni44 | 0.50 | <-6 | 8.9 | 400 | 1280 |