Inatumika kama vifaa kuu vya brazing ni AGCU7.5,AGCU25, AGCU28, AGCU55. Kwa sababu ya upinzani wa chini kwa mzigo wa muda mrefu chini ya joto la juu, inafaa tu kwa sehemu za brazing ambazo joto la kufanya kazi ni chini ya 400ºC.
Inatumika kama sarafu na mapambo. Aloi zinazotumiwa kama sarafu ni AGCU7.5, AGCU8,AGCU10, nk; Aloi zinazotumiwa kama mapambo ni AGCU8.4, AGCU12.5, nk
Ag | Cu | Sn | Ni | Pb | Fe | Sb | Bi | |
AGCU4 | 96 +/- 0.3 | 4+0.3/-0.5 | ≤0.005 | ≤0.05 | ≤0.002 | ≤0.002 | ||
AGCU5 | 95 +/- 0.3 | 5+0.3/-0.5 | ≤0.005 | ≤0.05 | ≤0.002 | ≤0.002 | ||
AGCU7.5 | 92.5 +/- 0.3 | 7.5+0.3/-0.5 | ≤0.005 | ≤0.1 | ≤0.002 | ≤0.002 | ||
AGCU8.4 | 91.6 +/- 0.3 | 8.4 +/- 0.5 | ≤0.005 | ≤0.1 | ≤0.002 | ≤0.002 | ||
AGCU10 | 90 +/- 0.3 | 10 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU12.5 | 87.5 +/- 0.3 | 12.5 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU20 | 80 +/- 0.3 | 20 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU23 | 77 +/- 0.5 | 23 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU25 | 75 +/- 0.5 | 25 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU26 | 74 +/- 0.5 | 26 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU28 | 72 +/- 0.5 | 28 +/- 0.5 | ≤0.005 | ≤0.2 | ≤0.002 | ≤0.002 | ||
AGCU50 | 50 +/- 0.5 | 50 +/- 0.5 | ≤0.005 | ≤0.25 | ≤0.002 | ≤0.002 | ||
AGCU99 | 1 +/- 0.2 | 99+0.2/-0.5 | ||||||
AGCU18NI2 | 80 +/- 0.5 | 18 +/- 0.5 | / | 2 +/- 0.3 |