Aloi za upinzani wa kupokanzwa wa shaba-nikeli na upinzani wa juu kwa kutu ya kemikali na oxidation na mgawo wa joto la chini, upinzani fulani wa umeme unaofikiwa na kujeruhiwa kwa waya kwenye koili na wakati huo huo unapita ndani yake - Joto linazalisha!
Maombi:
Daraja | CuNi44 | CuNi23 | CuNi10 | CuNi6 | CuNi2 | CuNi1 | CuNi8 | CuNi14 | CuNi19 | CuNi30 | CuNi34 | CuMn3 | |
Cuprothal | 49 | 30 | 15 | 10 | 5 | ||||||||
Isabellehutte | ISOTAN | Aloi 180 | Aloi 90 | Aloi 60 | Aloi 30 | ISAYA 13 | |||||||
Utungaji mdogo% | Ni | 44 | 23 | 10 | 6 | 2 | 1 | 8 | 14 | 19 | 30 | 34 | - |
Cu | Bal | Bal | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. | Bal | Bal | Bal | Bal | |
Mn | 1 | 0.5 | 0.3 | - | - | - | - | 0.5 | 0.5 | 1.0 | 1.0 | 3.0 | |
Kiwango cha juu cha halijoto cha kufanya kazi (uΩ/m kwa 20°C) | 0.49 | 0.3 | 0.15 | 0.10 | 0.05 | 0.03 | 0.12 | 0.20 | 0.25 | 0.35 | 0.4 | 0.12 | |
Ustahimilivu (Ω/cmf kwa 68°F) | 295 | 180 | 90 | 60 | 30 | 15 | 72 | 120 | 150 | 210 | 240 | 72 | |
Kiwango cha juu cha halijoto cha kufanya kazi (°C) | 400 | 300 | 250 | 200 | 200 | 200 | 250 | 300 | 300 | 350 | 350 | 200 | |
Uzito (g/cm³) | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | |
TCR(×10-6/°C) | <-6 | <16 | <50 | <60 | <120 | <100 | <57 | <30 | <25 | <10 | <0 | <38 | |
Nguvu ya Mkazo (Mpa) | ≥420 | ≥350 | ≥290 | ≥250 | ≥220 | ≥210 | ≥270 | ≥310 | ≥340 | ≥400 | ≥400 | ≥290 | |
Kurefusha(%) | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | ≥25 | |
EMF dhidi ya Cu UV/°C(0~100°C) | -43 | -34 | -25 | -12 | -12 | -8 | 22 | -28 | -32 | -37 | -39 | - | |
Kiwango Myeyuko (°C) | 1280 | 1150 | 1100 | 1095 | 1090 | 1085 | 1097 | 1115 | 1135 | 1170 | 1180 | 1050 | |
Mali ya Magnetic | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo | yasiyo |
150 0000 2421